By optimizing the magnet’s composition, microstructure and surface treatment, our company has developed a series of low- weight- loss magnet , the weight loss of which can be ≤ 2mg/cm² after the corrosion HAST test(130 ℃,2.7atm,100% humidity,30days), which has reached industry leading level.